No. 506, West Section of Huanghe Avenue, Lanzhou New Area, China
alaric@lshengchang.com.cn
HOME
ABOUT
PRODUCT
APPLICATION AREAS
General machinery
Nuclear power
Oil&Gas
Precision electronics
Gas turbine
MATERIAL TYPE
Super alloy
Copper alloy
Titanium alloy
High-end parts products
EQUIPMENT
CONTACT US
HOME
ABOUT
PRODUCT
APPLICATION AREAS
General machinery
Nuclear power
Oil&Gas
Precision electronics
Gas turbine
MATERIAL TYPE
Super alloy
Copper alloy
Titanium alloy
High-end parts products
EQUIPMENT
CONTACT US
Call Us Now!
postmaster @lshengchang.com.cn
产品分类
Application field
General machinery
Nuclear power
Oil&Gas
Oil drilling products
Precision electronics
Precision Alloy
Gas turbine
Product Type
Superalloy
Monel400
N08120Plate
N08810Plate
High-end parts products
Copper alloy
Titanium Alloy
Application field
General machinery
Nuclear power
Oil&Gas
Oil drilling products
Precision electronics
Precision Alloy
Gas turbine
Product Type
Superalloy
Monel400
N08120Plate
N08810Plate
High-end parts products
Copper alloy
Titanium Alloy
一、执行标准
316奥氏体不锈钢遵循以下国际及行业标准:
国际通用标准:
AISI、ASTM(如ASTM A240/A240M-19)
UNS编号为S31600
日标:
JIS G4303-2005(对应型号SUS316)
二、化学成分
典型成分范围如下(单位:wt%):
元素
碳(C)
铬(Cr)
镍(Ni)
钼(Mo)
锰(Mn)
硅(Si)
硫(S)
磷(P)
含量
≤0.08
16-18
10-14
2-3
≤2.00
≤1.00
≤0.03
≤0.045
注:钼(Mo)显著提升耐点蚀性;碳含量控制影响抗晶间腐蚀能力。
三、核心特性
耐腐蚀性:
在氯化物环境(如海水、化工介质)中耐点蚀和缝隙腐蚀性能优于304不锈钢。
对硫酸、磷酸、有机酸等具有良好抗性。
高温性能:
短期使用温度可达800℃,长期建议不超过450℃以防止σ相析出。
加工性能:
冷变形塑性良好,可进行深冲、折弯等加工。
焊接工艺性能优秀,推荐使用316L焊材以减少碳化物析出风险。
四、物理与力学性能
物理性能:
密度:7.98 g/cm³
熔点:1370-1450℃
热导率(100℃):16 W/(m·K)
力学性能(固溶处理态):
抗拉强度:≥515 MPa
屈服强度:≥205 MPa
延伸率:≥40%
五、典型应用领域
化工与能源:储罐、反应釜、核燃料后处理设备。
海洋工程:海水淡化设备、船用管道、螺旋桨轴。
医疗与食品:手术器械、食品加工设备、无菌管道系统。
建筑与装饰:沿海建筑外立面、高端装饰件。
六、衍生型号对比
316L:碳含量≤0.03%,抗晶间腐蚀能力更强,适用于焊接场景。
316H:碳含量0.04-0.10%,高温强度更高,用于锅炉及高温承压部件。
316N:添加氮元素(0.10-0.16%),增强强度同时保持耐蚀性。
Related products
Read more
Uncategorized
TA7
Read more
Uncategorized
Incoloy 825
Read more
Uncategorized
ZG40Cr28Ni48W5Si2
Read more
Uncategorized
ZG35Cr24Ni7SiN
English
Chinese